ABS Toyolac® 700 RD TORAY MALAYSIA
41
- Properties:High gloss
- Usages:Electrical appliancesToyMonitor
- Certificates:UL
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 18 kJ/m² |
| Impact strength of cantilever beam gap | -30°C,3.20mm | ASTM D256 | 110 J/m |
| -30°C,12.7mm | ASTM D256 | 80 J/m | |
| 0°C,3.20mm | ASTM D256 | 160 J/m | |
| 23°C,12.7mm | ASTM D256 | 200 J/m | |
| 0°C,12.7mm | ASTM D256 | 110 J/m | |
| 23°C,3.20mm | ASTM D256 | 220 J/m |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| bending strength | ASTM D790 | 73.0 Mpa | |
| ISO 178 | 77.0 Mpa | ||
| Bending modulus | ASTM D790 | 2300 Mpa | |
| tensile strength | Yield | ISO 527-2/50 | 51.0 Mpa |
| elongation | Break | ASTM D638 | 15 % |
| Tensile strain | Break | ISO 527-2/50 | >10 % |
| Tensile modulus | ISO 527-2/1 | 2600 Mpa | |
| tensile strength | Yield | ASTM D638 | 46.0 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| thermal conductivity | ASTMC177 | 0.16 W/m/K | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 7.2E-05 cm/cm/°C |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 81.0 °C |
| 1.8MPa,Unannealed,12.7mm | ASTM D648 | 92.0 °C | |
| 1.8MPa,Unannealed,6.40mm | ASTM D648 | 86.0 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 40 g/10min |
| density | ISO 1183 | 1.04 g/cm³ | |
| ASTM D792 | 1.05 g/cm³ | ||
| Water absorption rate | 23°C,24hr | ASTM D570 | 0.30 % |
| Shrinkage rate | MD | ASTM D955 | 0.40-0.60 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Dielectric constant | 1kHz | ASTM D150 | 3.10 |
| Dielectric strength | ASTM D149 | 23 KV/mm | |
| Volume resistivity | 23°C | ASTM D257 | >1.0E+16 ohms·cm |
| Surface resistivity | ASTM D257 | >1.0E+16 ohms | |
| Dissipation factor | 1kHz | ASTM D150 | 6.2E-03 |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 114 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.