PA66 EMLON® 66 GFR 35

0
  • Properties:
    Fillers
    glass fiber reinforced materials

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO11831.38到1.42 g/cm³
Shrinkage rate0.20到0.30 %
densityISO11831.38到1.42 g/cm³
Shrinkage rate0.20到0.45 %
hardnessTest ConditionTest MethodTest Result
ISO86880到85
ISO86875到85
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO527-210000到12000 MPa
Tensile stressYieldISO527-2170到210 MPa
Tensile strainBreakISO527-2>3.0 %
Tensile modulusISO527-28000到11000 MPa
Tensile stressYieldISO527-2170到220 MPa
Tensile strainBreakISO527-2>3.0 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO180/1A>8.0 kJ/m²
Impact strength of cantilever beam gapISO180/1A>7.0 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
ISO75-2/A250 °C
vicatISO306/B255 °C
ISO3146265 °C
ISO75-2/A250 °C
vicatISO306/B255 °C
ISO3146265 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.