Share
Add to Compare

PPS OCL-4536 BK SABIC INNOVATIVE US

127

Form:Granules | Grade:Injection grade

Properties:
Thermal stabilityFlame retardantFiller: Carbon fiber rein30%Filler by weight
Typical Applications:
Automotive componentsElectronic and electrical accessories
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:Automotive components | Electronic and electrical accessories
Properties:Thermal stability | Flame retardant | Filler: Carbon fiber rein | 30% | Filler by weight

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap23°CISO 180/1A3.2kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U14kJ/m²
Dart impact23°C,EnergyatPeakLoadASTM D37636.30J
Multi axis Instrumented Impact EnergyISO 6603-21.50J
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
bending strengthASTM D790230Mpa
Bending modulusISO 17819000Mpa
Bending modulusASTM D79020100Mpa
Tensile strainBreakISO 527-20.78%
elongationBreakASTM D6381.6%
Tensile strainYieldISO 527-20.77%
elongationYieldASTM D6380.90%
tensile strengthBreakISO 527-2113Mpa
tensile strengthBreakASTM D638119Mpa
tensile strengthYieldISO 527-2113Mpa
tensile strengthYieldASTM D638128Mpa
Tensile modulusISO 527-2/119900Mpa
Tensile modulusASTM D63818600Mpa
bending strengthISO 178176Mpa
Friction coefficientDynamicASTM D3702Modified0.36
Friction coefficientStaticASTM D3702Modified0.30
Wear factorWasherASTM D3702Modified15.010^-10in^5-min/ft-lb-hr
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionTD:-40to40°CISO 11359-27E-06cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CASTME8317.2E-06cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CISO 11359-23.6E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8313.6E-05cm/cm/°C
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpanISO 75-2/Af248°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D648259°C
Hot deformation temperature0.45MPa,Unannealed,64.0mmSpanISO 75-2/Bf272°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTM D648274°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Shrinkage rateMD:24hrISO 294-40.15%
Shrinkage rateTD:24hrISO 294-40.66%
Shrinkage rateTD:24hrASTM D9550.70%
Shrinkage rateMD:24hrASTM D9550.20%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China