物理性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
密度 | 本色混合物 | ASTMD792 | 0.941 g/cm³ |
熔体质量流动速率 | 190°C/2.16kg2 | ASTMD1238 | 0.16 g/10min |
190°C/21.6kg3 | ASTMD1238 | 9.5 g/10min |
机械性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
SlowCrackGrowthResistance | PENT4 | ASTMF1473 | 15000 hr |
抗快速裂缝扩展,Pc | S-4:0°C7 | ISO13477 | >10.0 bar |
已计算,全刻度:0°C8 | ISO13478 | >38.6 bar | |
抗快速裂缝扩展,Tc-S- | ISO13477 | <-2 °C | |
抗张强度 | Yield | ASTMD638 | >17.9 MPa |
伸长率 | Break | ASTMD638 | >600 % |
弯曲模量 | ASTMD790B | >621 MPa | |
SlowCrackGrowthResistance | NotchedPipeTest6 | ISO13479 | >3000 hr |
热性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
脆化温度 | ASTMD746A | <-75.0 °C | |
热稳定性 | ASTMD3350 | >220 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.