PP ADDILENE H 590 RM20 F ADDIPLAST FRANCE
Properties:
Filler ADDIPLAST French ADDIPLAST
Typical Applications:
Home appliance components electrical and electronic application fields
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Home appliance components | electrical and electronic application fields |
| Properties: | Filler | ADDIPLAST | French ADDIPLAST |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | ISO 180/1A | 3.8 | kJ/m² | |
| Impact strength of simply supported beam without notch | ISO 179/1eU | 38 | kJ/m² | |
| Charpy Notched Impact Strength | ISO 179/1eA | 3.0 | kJ/m² | |
| ISO 179/1eA | 3.0 | kJ/m² | ||
| Impact strength of simply supported beam without notch | ISO 179/1eU | 38 | kJ/m² | |
| Impact strength of cantilever beam gap | ISO 180/1A | 3.8 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.6mm | UL 94 | V-0 | |
| Extreme Oxygen Index | ISO 4589-2 | 26 | % | |
| Hot filament ignition temperature | IEC 60695-2-13 | 960 | °C | |
| UL flame retardant rating | 1.6mm | UL 94 | V-0 | |
| Hot filament ignition temperature | IEC 60695-2-13 | 960 | °C | |
| Extreme Oxygen Index | ISO 4589-2 | 26 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ISO 178 | 2400 | MPa | |
| Tensile strain | Break | ISO 527-2 | 50 | % |
| tensile strength | Break | ISO 527-2 | 20.0 | MPa |
| Break | ISO 527-2 | 20.0 | MPa | |
| Tensile strain | Break | ISO 527-2 | 50 | % |
| Bending modulus | ISO 178 | 2400 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ISO 306/A50 | 140 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/Af | 70.0 | °C |
| Melting temperature | ISO 3146 | 165 | °C | |
| ISO 3146 | 165 | °C | ||
| Vicat softening temperature | ISO 306/A50 | 140 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/Af | 70.0 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 18 | g/10min |
| density | ISO 1183/A | 1.34 | g/cm³ | |
| ISO 1183/A | 1.34 | g/cm³ | ||
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 18 | g/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 | |
| Dielectric strength | IEC 60243-1 | 43 | kV/mm | |
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 | |
| Dielectric strength | IEC 60243-1 | 43 | kV/mm | |
| Volume resistivity | IEC 60093 | 1E+15 | ohms·cm | |
| Surface resistivity | IEC 60093 | 1E+13 | ohms | |
| IEC 60093 | 1E+13 | ohms | ||
| Volume resistivity | IEC 60093 | 1E+15 | ohms·cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD | ISO 868 | 67 | |
| ShoreD | ISO 868 | 67 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.