PA6 BG-15 S EMS-CHEMIE SWITZERLAND
221
Form:Granules | Grade:Enhanced level
Properties:
High impact resistanceGlass fiber reinforcedFiller: Glass fiber reinf15%Filler by weight
Typical Applications:
Electrical fieldElectronic fieldHome appliance componentsAutomotive sectorAutomotive interior partsElectrical/Electronic ApplicationsApplication in the automotive fieldHome appliance componentsAutomotive interior parts
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Electrical field | Electronic field | Home appliance components | Automotive sector | Automotive interior parts | Electrical/Electronic Applications | Application in the automotive field | Home appliance components | Automotive interior parts |
| Properties: | High impact resistance | Glass fiber reinforced | Filler: Glass fiber reinf | 15% | Filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | kJ/m² | 45 | 85 |
| -30°C | kJ/m² | 40 | 45 | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Flammability level | 0.8mm | HB | -- | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break | % | 4.0 | |
| tensile strength | Break | MPa | 140 | 75.0 |
| Tensile modulus | MPa | 6700 | 3400 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | °C | 222 | -- | |
| Continuous use temperature | --4 | °C | 160 | -- |
| --3 | °C | 90.0to110 | -- | |
| Linear coefficient of thermal expansion | TD | cm/cm/°C | 1.2E-04 | -- |
| MD | cm/cm/°C | 5E-05 | -- | |
| Hot deformation temperature | 1.8MPa,Unannealed | °C | 195 | -- |
| 8.0MPa,Unannealed | °C | 60.0 | -- | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | % | 2.5 | -- |
| Saturation,23°C | % | 8.0 | -- | |
| Shrinkage rate | MD | % | 0.10 | -- |
| TD | % | 0.60 | -- | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | ohms | -- | 1E+12 | |
| Dielectric strength | kV/mm | 40 | 37 | |
| Volume resistivity | ohms·cm | 1E+14 | 1E+13 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | MPa | 170 | 80.0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.