Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Apparent density | | | 0.59 g/cm³ |
Melt volume flow rate | | ISO1133 | 2.00 cm3/10min |
Melt volume flow rate | | ISO1133 | 17.0 cm3/10min |
Shrinkage rate | | ISO294-4 | 0.40to0.70 % |
Water absorption rate | | ISO62 | 0.70 % |
hardness | Test Condition | Test Method | Test Result |
---|
| | ISO2039-1 | 70.0 Mpa |
optical performance | Test Condition | Test Method | Test Result |
---|
refractive index | | ISO489 | 1.540 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile creep modulus | | ISO899-1 | 1250 Mpa |
Bending stress | | ISO178 | 70.0 Mpa |
Tensile modulus | | ISO527-2 | 2000 Mpa |
Tensile stress | | ISO527-2 | 48.0 Mpa |
Tensile strain | | ISO527-2 | 4.0 % |
Nominal tensile fracture strain | | ISO527-2 | 12 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of simply supported beam without notch | | ISO179 | 80 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179 | 120 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | IEC60093 | 1E+15 ohms |
Volume resistivity | | IEC60093 | 1E+15 ohms·cm |
dielectric constant | | IEC60250 | 2.90 |
Dissipation Factor | | IEC60250 | 0.016 |
Dissipation Factor | | IEC60250 | 0.014 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Hot deformation temperature 3 | | ISO75-2/B | 94.0 °C |
Hot deformation temperature 3 | | ISO75-2/A | 90.0 °C |
vicat | | ISO306/A50 | 105 °C |
vicat | | ISO306/B50 | 93.0 °C |
| | ISO11359-2 | 8.0E-5to1.1E-4 cm/cm/°C |
thermal conductivity | | DIN52612 | 0.17 W/m/K |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.