Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD3575 | 0.0481 g/cm³ | |
VOCContent | 5.5 % | ||
0.30 % | |||
0.900到2.00 mm |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
Puncture | ASTMD3763 | 432 N | |
Tear strength - atMaximmLoad | ASTMD3575 | 3.9 kN/m |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
compressive strength | ASTMD3575 | 0.380 MPa | |
ASTMD3575 | 0.462 MPa | ||
tensile strength | Break | ASTMD3575 | 0.650 MPa |
bending strength | ASTMC203 | 0.699 MPa | |
ASTMC203 | 0.740 MPa | ||
compressive strength | ASTMD3575 | 0.330 MPa | |
ASTMD3575 | 0.957 MPa | ||
Bending Strain | ASTMC203 | 8.4 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.