Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Resistance to environmental stress cracking | | ASTMD1693B | >1000 hr |
density | | ASTMD4883 | 0.950 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 9.0 g/10min |
Resistance to environmental stress cracking | | ASTMD1693A | 430 hr |
Resistance to environmental stress cracking | | ASTMD1693B | 340 hr |
Resistance to environmental stress cracking | | ASTMD1693A | >1000 hr |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 63 |
Impact resistance | Test Condition | Test Method | Test Result |
---|
NotchedIzodImpact | | ASTMD256 | 44.0 kJ/m² |
InstrumentedImpact,Ductility | | ASTMD3763 | Ductile |
Impact strength of cantilever beam gap | | ASTMD256 | 450 J/m |
InstrumentedImpact,Ductility | | ASTMD3763 | Ductile |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Yield | ASTMD638 | 26.2 MPa |
tensile strength | Break | ASTMD638 | 37.2 MPa |
elongation | Yield | ASTMD638 | 9.9 % |
elongation | Break | ASTMD638 | 850 % |
Flexural modulus | | ASTMD790A | 917 MPa |
Flexural modulus | Tangent | ASTMD790A | 1230 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 70.0 °C |
| | ASTMD648 | 47.8 °C |
brittle temperature | | ASTMD746 | <-75.0 °C |
vicat | | ASTMD1525 | 126 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.