TPU-Ether Quadraflex™ ARE-75A-B20

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
Post curing time6.0to10 hr
physical property Test ConditionTest MethodTest Result
densityASTM D7921.23 g/cm³
melt mass-flow rateASTM D12387.5 g/10min
Shrinkage rateASTM D9550.80to1.2 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore AASTM D224075
Mechanical propertiesTest ConditionTest MethodTest Result
Flexural modulusASTM D7905.52 MPa
elastomerTest ConditionTest MethodTest Result
elongationBreakASTM D412550 %
tensile strength ASTM D4123.28 MPa
tensile strength ASTM D4123.79 MPa
tensile strength ASTM D4129.65 MPa
tensile strength BreakASTM D41234.5 MPa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.