Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | ASTMD955 | 0.74 % |
Shrinkage rate | | ASTMD955 | 1.4 % |
Shrinkage rate | | ISO294-4 | 1.4 % |
Shrinkage rate | | ISO294-4 | 0.74 % |
density | | ASTMD792 | 1.05 g/cm³ |
density | | ISO1183 | 1.21 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | R-Scale | ASTMD785 | 110 |
Rockwell hardness | R-Scale | ISO2039-2 | 110 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD638 | 98.1 MPa |
tensile strength | | ISO527-2 | 115 MPa |
elongation | Break | ASTMD638 | 2.0 % |
elongation | Break | ISO527-2 | 3.0 % |
Flexural modulus | | ASTMD790 | 4710 MPa |
Flexural modulus | | ISO178 | 4400 MPa |
bending strength | | ASTMD790 | 162 MPa |
bending strength | | ISO178 | 175 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO179/1eA | 6.0 kJ/m² |
Impact strength of cantilever beam gap | | ASTMD256 | 68 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 225 °C |
| | ISO75-2/A | 220 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.