Technical Data Sheet

physical property Test ConditionTest MethodTest Result
density内部方法0.900to0.930 g/cm³
melt mass-flow rateISO 11338.0to12 g/10min
hardnessTest ConditionTest MethodTest Result
Shore hardnessISO 868>62
Supplementary InformationTest ConditionTest MethodTest Result
ChargeRate0.0to2.0 %
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldISO 527-2>20.0 MPa
tensile strength BreakISO 527-2>11.0 MPa
Tensile strainBreakISO 527-2>25 %
Flexural modulusISO 178950 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180>7.0 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/A>48.0 °C
vicatISO 306/A>120 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.