Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
Thermosetting components | 100 | ||
按重量计算的混合比:53 |
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
MoldedDensity | ASTM D3574A | 144 kg/m³ |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D3574E | 0.324 MPa | |
ASTM D3574K | 0.124 MPa | ||
elongation | Break | ASTM D3574E | 44 % |
ASTM D3574K | 17 % |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
compression set | ASTM D3574D | 14 % | |
ASTM D3574D | 18 % | ||
tear strength | ASTM D3574F | 0.175 kN/m | |
CompressionForceDeflection | ASTM D3574C | 0.179 MPa | |
ASTM D3574C | 0.117 MPa | ||
compression set | ASTM D3574D | 29 % | |
ASTM D3574D | 36 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.