PC/ABS NS0031 BK2D038 SABIC INNOVATIVE US
37
Form:Granules | Grade:Injection grade
Properties:
High mobilityFlame retardant
Typical Applications:
CastersElectrical applications
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Casters | Electrical applications |
| Properties: | High mobility | Flame retardant |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 9.5 | kJ/m² |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 32 | kJ/m² |
| Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 15.0 | J |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ASTM D638 | 3110 | Mpa | |
| ISO 527-2/1 | 2700 | Mpa | ||
| tensile strength | Yield | ASTM D638 | 52.4 | Mpa |
| Yield | ISO 527-2 | 50.0 | Mpa | |
| Break | ASTM D638 | 49.6 | Mpa | |
| Break | ISO 527-2 | 46.0 | Mpa | |
| elongation | Yield | ASTM D638 | 3.3 | % |
| Tensile strain | Yield | ISO 527-2 | 3.5 | % |
| elongation | Break | ASTM D638 | 4.7 | % |
| Tensile strain | Break | ISO 527-2 | 6.0 | % |
| Bending modulus | ASTM D790 | 2990 | Mpa | |
| ISO 178 | 2800 | Mpa | ||
| bending strength | ASTM D790 | 89.6 | Mpa | |
| ISO 178 | 86.0 | Mpa | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO 75-2/Bf | 115 | °C |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | 105 | °C | |
| 1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 103 | °C | |
| Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7.7E-05 | cm/cm/°C |
| MD:-40to40°C | ISO 11359-2 | 5.9E-05 | cm/cm/°C | |
| TD:-40to40°C | ASTME831 | 6.3E-05 | cm/cm/°C | |
| TD:-40to40°C | ISO 11359-2 | 8.2E-05 | cm/cm/°C | |
| Hot deformation temperature | 0.45MPa,Unannealed,3.20mm | ASTM D648 | 120 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | MD:24hr | ASTM D955 | 0.30 | % |
| TD:24hr | ASTM D955 | 0.35 | % | |
| TD:24hr | ISO 294-4 | 0.35 | % | |
| MD:24hr | ISO 294-4 | 0.30 | % | |
| Water absorption rate | 24hr,50%RH | ASTM D570 | 0.10 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | ASTM D257 | 10to1.0E+3 | ohms | |
| Volume resistivity | ASTM D257 | 1E+04 | ohms·cm | |
| Shielding effectiveness (EMI) | 3.00mm | Internal Method | 50to65 | dB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.