physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD1505 | 0.927 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 0.80 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|
gloss | | ASTMD2457 | 85 |
elastomer | Test Condition | Test Method | Test Result |
---|
tear strength | | ASTMD1004 | 152 kN/m |
tear strength | | ASTMD1004 | 142 kN/m |
film | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD882 | 57.9 MPa |
tensile strength | | ASTMD882 | 53.0 MPa |
elongation | | ASTMD882 | 600 % |
elongation | | ASTMD882 | 630 % |
Falling hammer impact | | ASTMD1709A | 250 g |
| | 内部方法 | 120 °C |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ASTMD1525 | 120 °C |
| | ASTMD3418 | 122 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.