TPE 1170

0
  • Properties:
    Injection molding reference process feeding section temperature
    150-160 ℃
    model temperature
    10-50 ℃
    middle section temperature
    170-190 ℃
    screw speed
    100-200r
    min
    front section temperature
    180-220 ℃
    back pressure
    0
    1-1
    0MPa
    nozzle temperature
    180-230 ℃
    injection pressure
    medium high MPa
    extrusion reference process barrel feeding section temperature 130-150?

Technical Data Sheet

Basic performanceTest ConditionTest MethodTest Result
relative density0.97 g/cm
Mechanical propertiesTest ConditionTest MethodTest Result
Shore hardness70 A
tear strength31.5 kN/m
Elongation730 %
stretching strength1.8 MPa
tensile strength 8.5 MPa
Other performanceTest ConditionTest MethodTest Result
Retention rate of elongation at break98 %
Tensile strength retention rate104 %
compression set28
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.