TPU-Ester Texalan® 4 Series 472D Austin Novel Materials Co., Ltd.

0

Technical Data Sheet

elastomerTest ConditionTest MethodTest Result
tensile strength300%StrainISO 37>42.0 MPa
Permanent compression deformation70°CISO 815<40 %
tear strengthISO 34-1>190 kN/m
elongationBreakISO 37>350 %
tensile strengthYieldISO 37>55.0 MPa
tensile strength100%StrainISO 37>30.0 MPa
mechanical propertiesTest ConditionTest MethodTest Result
Wear resistanceISO 4649<30.0 mm³
Physical propertiesTest ConditionTest MethodTest Result
densityISO 11831.20to1.24 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreDISO 761969to75
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.