Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 0.900 g/cm³ |
Apparent density | | | 0.48到0.60 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 10到15 g/10min |
Ash Content | | | 0.025到0.050 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | R-Scale | | 40到88 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
ThermalCreepTemperature | | | 64到90 °C |
Thermal-oxidativeDeterioration | | | 15.0 day |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Flexural modulus | | ASTMD790 | 1200 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 45 J/m |
Impact strength of cantilever beam gap | | ASTMD256 | 120 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | | 126到150 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.