PA66 K224-G6 DSM HOLAND
148
Form:Granules | Grade:Enhanced level
Properties:
Glass fiber reinforcedFiller: Glass fiber reinf30%Filler by weight
Typical Applications:
Insulation materialShellfurniturewheel
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Insulation material | Shell | furniture | wheel |
| Properties: | Glass fiber reinforced | Filler: Glass fiber reinf | 30% | Filler by weight |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 90 | kJ/m² |
| -30°C | ISO 179/1eU | 75 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Hot filament ignition temperature | 1.5mm | IEC 60695-2-13 | 725 | °C |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 700 | °C |
| 1.5mm | IEC 60695-2-12 | 700 | °C | |
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | HB | |
| 0.75mm | IEC 60695-11-10,-20 | HB | ||
| Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 725 | °C |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break | ISO 527-2 | 3.5 | % |
| tensile strength | Break | ISO 527-2 | 180 | Mpa |
| Tensile modulus | ISO 527-2 | 9500 | Mpa | |
| bending strength | ISO 178 | 235 | Mpa | |
| Bending modulus | ISO 178 | 8600 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 2E-05 | cm/cm/°C |
| Melting temperature | ISO 11357-3 | 220 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 200 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 220 | °C | |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 7E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 1.9 | % |
| Saturation,23°C | ISO 62 | 6.3 | % | |
| Shrinkage rate | MD | ISO 294-4 | 0.30 | % |
| TD | ISO 294-4 | 0.90 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 1MHz | IEC 60250 | 0.015 | |
| 100Hz | IEC 60250 | 5E-03 | ||
| Relative permittivity | 1MHz | IEC 60250 | 3.30 | |
| 100Hz | IEC 60250 | 3.50 | ||
| Surface resistivity | IEC 60093 | -- | ohms | |
| Volume resistivity | IEC 60093 | 1E+15 | ohms·cm | |
| Dielectric strength | IEC 60243-1 | 30 | KV/mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.