LCP E6008LMR B SUMITOMO JAPAN
181
Form:Granules | Grade:Injection grade
Properties:
dimensional stability Low warpageLow viscosityHigh rigidityGood forming performanceWeldableAging resistanceGood adhesionChemical resistanceheat-resistingGlass fiber reinforcedhigh strength
Typical Applications:
Electrical appliancesAutomotive sectorElectronic fieldEngineering accessoriesFood containersHousehold appliancesHousehold appliancesAutomotive sector
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Electrical appliances | Automotive sector | Electronic field | Engineering accessories | Food containers | Household appliances | Household appliances | Automotive sector |
| Properties: | dimensional stability | Low warpage | Low viscosity | High rigidity | Good forming performance | Weldable | Aging resistance | Good adhesion | Chemical resistance | heat-resisting | Glass fiber reinforced | high strength |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Suspended wall beam without notch impact strength | 6.40 mm | ASTM D256 | 410 | J/m |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | ISO 527-1 | 48 | % | |
| UL flame retardant rating | 0.30 mm | UL 94 | V-0 | |
| Solder resistance | Internal Method | 300 | °C | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | ASTM D638 | 147 | Mpa | |
| Bending modulus | 23°C | ASTM D790 | 12300 | Mpa |
| elongation | Break | ASTM D638 | 5.2 | % |
| Poisson's ratio | ASTM D785 | 0.46 | ||
| shear strength | ASTM D732 | 51.0 | Mpa | |
| bending strength | 200°C | ASTM D790 | 33.0 | Mpa |
| 23°C | ASTM D790 | 143 | Mpa | |
| Bending modulus | 200°C | ASTM D790 | 4900 | Mpa |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Processing (melt) temperature | 360 | °C | ||
| Mold temperature | 40 to 160 | °C | ||
| Temperature at the front of the material cylinder | 340 to 370 | °C | ||
| Spray nozzle temperature | 340 to 370 | °C | ||
| drying time | 4.0 to 24 | hr | ||
| Temperature at the rear of the barrel | 280 to 320 | °C | ||
| Back pressure | 1.00 to 5.00 | Mpa | ||
| Screw speed | 50 to 100 | rpm | ||
| Injection pressure | 80.0 to 160 | Mpa | ||
| Injection speed | 中等偏快 | |||
| Maintain pressure | 20.0 to 40.0 | Mpa | ||
| Temperature in the middle of the barrel | 320 to 350 | °C | ||
| drying temperature | 130 | °C | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | Across Flow : 150°C | Internal Method | 5.6E-5 | cm/cm/°C |
| Flow : 150°C | Internal Method | 1.3E-5 | cm/cm/°C | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 279 | °C |
| thermal conductivity | JIS R2618 | 0.52 | W/m/K | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | 横向Flow | Internal Method | 1.2 | % |
| Flow | Internal Method | 0.18 | % | |
| Water absorption rate | Saturation | ASTM D570 | 0.020 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | 1 MHz | ASTM D150 | 3.90 | |
| Arc resistance | ASTM D495 | 130 | sec | |
| Dissipation factor | 1 kHz | ASTM D150 | 0.022 | |
| Volume resistivity | ASTM D257 | 1.0E+15 | ohms·cm | |
| Dielectric constant | 1 kHz | ASTM D150 | 4.40 | |
| Dissipation factor | 1 MHz | ASTM D150 | 0.022 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 103 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.