Technical Data Sheet

elastomerTest ConditionTest MethodTest Result
tensile strength100%StrainASTM D4121.00 MPa
tensile strength300%StrainASTM D4122.00 MPa
tensile strengthBreakASTM D4127.50 MPa
elongationBreakASTM D412>750 %
Permanent compression deformationASTM D395B15 %
thermal performanceTest ConditionTest MethodTest Result
Brittle temperatureASTM D2137-55.0 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7920.900 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreAASTM D224043to47
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.