Share
Add to compare

SEBS HP65 EMPILON

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

elastomerTest ConditionTest MethodTest ResultTest Unit
tensile strengthASTM D4127.06MPa
tensile strength300%StrainASTM D4124.12MPa
Permanent compression deformation23°C,70hrASTM D39519%
elongationBreakASTM D412570%
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Brittle temperature-40.0°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Shrinkage rateTD1.0%
Shrinkage rateMD1.0%
melt mass-flow rate200°C/5.0kgASTM D12386.0g/10min
densityASTM D7921.10g/cm³
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreA,10SecASTM D224061
agingTest ConditionTest MethodTest ResultTest Unit
Change rate of hardness (Shore) in the airShoreA,125°C,168hrASTM D5734.0
Change rate of ultimate elongation in air125°C,168hrASTM D5732.0%
Change rate of tensile strength in air125°C,168hrASTM D573-10%
Supplementary InformationTest ConditionTest MethodTest ResultTest Unit
Adhesion to ABS3.5kN/m
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.