Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.45 g/cm³ |
Water absorption rate | | ASTMD570 | 1.5 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-0 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
bending strength | | ASTMD790 | 130 MPa |
bending strength | | ASTMD790 | 92.4 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 26 J/m |
Impact strength of cantilever beam gap | | ASTMD256 | 28 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
High Voltage Arc Traceability Rate (HVTR) | | UL746 | 1.90 mm/min |
Hot wire ignition (HWI) | | UL746 | 63 sec |
DielectricBreakdown | | ASTMD149 | 45000 V |
dielectric strength | | ASTMD149 | >18 kV/mm |
arc resistance | | ASTMD495 | 123 sec |
Compared to the Leakage Tracking Index (CTI) | | UL746 | >500 V |
High arc combustion index (HAI) | | UL746 | >200 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
RTI Elec | | UL746 | 50.0 °C |
RTI | | UL746 | 50.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.