TSU 352 (76A)

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
按重量计算的混合比:5.0
按重量计算的混合比:33
按重量计算的混合比:100
hardnessTest ConditionTest MethodTest Result
Shore AASTMD224076
Mechanical propertiesTest ConditionTest MethodTest Result
ASTMD348937.0 mg
elastomerTest ConditionTest MethodTest Result
tensile strengthBreakASTMD41216.6 MPa
elongationBreakASTMD412410 %
tear strengthASTMD62447.8 kN/m
tear strengthSplitASTMD193813 kN/m
compression setASTMD395B84 %
Basho elasticityASTMD263233 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.