PA612 Zytel® 77G33L DUPONT USA
444
- Properties:wear resistantHigh impact resistance
- Usages:Automotive ApplicationsFitness equipmentelectrical equipment
- Certificates:UL
Technical Data Sheet
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Fracture stress | ISO 527 | 168 | Mpa | |
Fracture strain | ISO 527 | 3 | % | |
Tensile modulus | ISO 527 | 9500 | Mpa | |
Bending modulus | ISO 178 | 8200 | Mpa | |
Charpy notch impact strength | -40 ℃ | ISO 179/1eA | 12 | kJ/m² |
-30℃ | ISO 179/1eA | 11 | kJ/m² | |
23 ℃ | ISO 179/1eA | 13 | kJ/m² | |
Impact strength of simply supported beam without notch | -30℃ | ISO 179/1eU | 60 | kJ/m² |
23 ℃ | ISO 179/1eU | 80 | kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa | ASTM D790/ISO 178 | 216 | °C |
1.80MPa | ASTM D790/ISO 178 | 200 | °C | |
Melting temperature | 10°C/min | ISO 11357-1/-3 | 218 | °C |
Linear coefficient of thermal expansion | Normal | ISO 11359-1/-2 | 0.83 | E-4/C |
Parallel | ISO 11359-1/-2 | 0.26 | E-4/C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume resistivity | IEC 60093 | 1E+13 | E-4/C | |
Resistance to conductive tracks | 3.0mm | UL 746A | >550 | V |
Flame retardant grade | 0.75mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.