PA6 BKV30H2.0 901510 ENVALIOR WUXI
31
- Properties:30% glass fiber reinforceEasy to flowThermal stability rating
Technical Data Sheet
processability | Test Condition | Test Method | Test Result |
---|---|---|---|
injection speed | ISO 294 | 200 mm/s | |
Temperature | ISO 294 | 80 °C | |
Melt Temperature | ISO 294 | 280 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Bending stress at 3.5% strain | ISO 178 | 250 Mpa | |
Charpy notch impact strength | ISO 179-1eA | <10 kJ/m² | |
tensile strength | ISO 527-1,-2 | 170 Mpa | |
Elongation | ISO 527-1,-2 | 3.2 % | |
ISO 178 | 4.1 % | ||
Tensile modulus | ISO 527-1,-2 | 9000 Mpa | |
bending strength | ISO 178 | 260 Mpa | |
Flexural modulus | ISO 178 | 8000 Mpa |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Glass Fiber Content | ISO 3451-1 | 30 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
ISO 75-1,-2 | 150 °C | ||
Hot deformation temperature method Af | ISO 75-1,-2 | 200 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.