Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
OilContent-HI-AR | ASTMD5774 | 14到17 % | |
Organic Acid | ASTMD5774 | 5.0到6.7 % | |
Soap-OrganicAcid | ASTMD5774 | <0.30 % | |
Ash Content | ASTMD5667 | <0.60 % | |
Volatile compounds | ASTMD5668 | <0.60 % | |
Mooney viscosity | ASTMD1646 | 46到56 MU | |
Bound styrene | 内部方法 | 21.0到24.0 % |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile stress | ASTMD3185 | >9.80 MPa | |
tensile strength | Yield | ASTMD3185 | >21.6 MPa |
elongation | Break | ASTMD3185 | 400到650 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.