物理性能 | Test Condition | Test Method | Test Result |
---|
收缩率 | 流动 | ASTM D955 | 0.2 % |
收缩率 | 横向 | ASTM D955 | 0.4 % |
热性能 | Test Condition | Test Method | Test Result |
---|
溶融温度 | | ASTM D3418 | 310 °C |
热变形温度 | 1.8MPa,退火, | ASTM D648 | 277 °C |
电气性能 | Test Condition | Test Method | Test Result |
---|
介质损耗因数 | 1MHZ | ASTM D150 | 0.011 |
体积电阻率 | | ASTM D257 | 1E+15 ohm*cm |
电气强度 | | ASTM D149 | 23 KV/mm |
介电常数 | 1MHZ | ASTM D150 | 4.10 |
机械性能 | Test Condition | Test Method | Test Result |
---|
拉伸模量 | | ASTM D638 | -- Mpa |
拉伸应力 | | ASTM D527-2 | 193 Mpa |
拉伸伸长率 | break | ASTM D638 | 1.5 % |
弯曲模量 | | ASTM D790 | 15500 Mpa |
弯曲强度 | | ASTM D790 | 276 Mpa |
Charpy缺口冲击强度 | 23℃ | ISO 179/1eA | 7.8 kJ/m² |
Charpy缺口冲击强度 | 23℃ | ISO 179/1eU | 33.1 kJ/m² |
缺口冲击强度 | | ASTM D256 | 107 J/m |
其它 | Test Condition | Test Method | Test Result |
---|
UL阻燃等级 | 0.794mm | UL 94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.