PP Homopolymer Advanced-PP 1101P

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO11830.910 g/cm³
Water absorptionISO620.10 %
Water absorptionISO620.10 %
ISO113326 g/10min
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ISO527-235 MPa
elongation at breakISO527-2>=10 %
elongation at breakISO527-250 %
Tensile modulusISO527-21550 MPa
Charpy Notched Impact StrengthISO179/1eA3.0 kJ/m²
Charpy Notched Impact StrengthISO179/1eA1.5 kJ/m²
Impact strength of simply supported beam without notchISO179/1eU105 kJ/m²
Impact strength of simply supported beam without notchISO179/1eU15 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
IEC60093>=1.0E+15 Ω.cm
Surface ResistivityIEC600931E+14 Ω.cm
Dielectric StrengthIEC60243-1140 KV/mm
dielectric constantIEC602502.3 1MHz
Dissipation FactorIEC602500.00020 1MHz
Comparative Tracking IndexIEC60112600 V
Thermal performanceTest ConditionTest MethodTest Result
ISO11359-21.4E-04 cm/cm/°C
melting point163 °C
ISO75-2/Bf85 °C
ISO75-2/Af55 °C
vicatISO306/A5092 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.