ABS H-2938 KUMHO KOREA

105

Technical Data Sheet

mechanical propertiesTest ConditionTest MethodTest Result
Bending modulus23℃ASTM D-79023000(327100) kg/cm2 (lbf/in2)
Impact strength of cantilever beam gap1/4in(6.4mm) 23℃ASTM D-25618(3.3) kg.cm/cm(ft.1b/in)
bending strength23℃ASTM D-790700(9950) kg/cm2 (lbf/in2)
elongationASTM D-63825 %
tensile strength23℃ASTM D-638490(7000) kg/cm2 (lbf/in2)
Rockwell hardnessASTM D-785106 R
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperatureUnannealed,6.4mm 18.6kg/cm2ASTM D-64897(207) ℃(℉)
Hot deformation temperatureAnnealed,6.4mm 18.6kg/cm2ASTM D-648107(225) ℃(℉)
Vicat softening temperatureASTM D-1525115(239) ℃(℉)
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateASTM D-9550.4-0.7 %
melt mass-flow rate200℃ 5kg(条件G)ASTM D-12382.3 g/10min
melt mass-flow rate200℃ 21.6kg锦湖日丽标准10 g/10min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.