physical property Test ConditionTest MethodTest Result
densityASTMD7921.51 g/cm³
Shrinkage rateASTMD9550.30 %
Shrinkage rateASTMD9550.40 %
Water absorption rateASTMD5700.36 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTMD785134
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL94V-0
Impact resistanceTest ConditionTest MethodTest Result
Suspended wall beam without notch impact strengthASTMD256430 J/m
Impact strength of cantilever beam gapASTMD25680 J/m
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTMD638124 MPa
elongationBreakASTMD6383.0 %
Flexural modulusASTMD7905900 MPa
bending strengthASTMD790172 MPa
Electrical performanceTest ConditionTest MethodTest Result
arc resistanceASTMD495150 sec
Volume resistivityASTMD2571E+16 ohms·cm
Thermal performanceTest ConditionTest MethodTest Result
Heat Deflection TemperatureASTMD648210 °C
Linear thermal expansion coefficientASTMD6962.6E-05 cm/cm/°C
Linear thermal expansion coefficientASTMD6964.8E-05 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.