PUR-Ester Generic PUR-Ester

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.05到1.07 g/cm³
thermosettingTest ConditionTest MethodTest Result
Thermosetting mixed viscosityASTMD239350.0到238 cP
hardnessTest ConditionTest MethodTest Result
ASTMD224078到84
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTMD63839.3到77.3 MPa
Filling analysisTest ConditionTest MethodTest Result
melt viscosityASTMD38350.500到80.0 Pa·s
elastomerTest ConditionTest MethodTest Result
Tensile stressASTMD4120.981到20.7 MPa
tensile strengthASTMD4129.56到10.7 MPa
tensile strengthASTMD41230.0到53.9 MPa
elongationASTMD412500到800 %
filmTest ConditionTest MethodTest Result
tensile strengthISO527-333.8到50.0 MPa
elongationISO527-3400到570 %
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureASTME1356-46.5到-27.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.