Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.18 g/cm³ |
Water absorption rate | | ASTMD570 | 0.30 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 90到100 |
Barcol Hardness | | ASTMD2583 | 50 |
optical performance | Test Condition | Test Method | Test Result |
---|
refractive index | | ASTMD542 | 1.490 |
transmissivity | | ASTMD1003 | 70.0 % |
transmissivity | | ASTMD1003 | 90.0 % |
Haze ratio | | ASTMD1003 | 2.0 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 2930 MPa |
tensile strength | | ASTMD638 | 66.2 MPa |
elongation | | ASTMD638 | 4.5 % |
bending strength | | ASTMD790 | 103到110 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Suspended wall beam without notch impact strength | | ASTMD256 | 21到27 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Continuous use temperature | | ASTMD794 | 60.0 °C |
melting temperature | | | 140到180 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.