PA6 9B20400 4Plas
Properties:
Additive UV stabilizer characteristics good UV resistance processing method injection molding
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Additive | UV stabilizer characteristics | good UV resistance processing method | injection molding |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 6.0 | kJ/m² |
| -30°C | ISO 180/1A | 5.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.6mm | UL 94 | HB | |
| 3.2mm | UL 94 | HB | ||
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 750 | °C |
| UL flame retardant rating | 1.60 mm | UL 94 | HB | |
| 3.20 mm | UL 94 | HB | ||
| Burning wire flammability index | 2.00 mm | IEC 60695-2-12 | 750 | °C |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break,23°C | ISO 527-2/5 | 35 | % |
| tensile strength | Break,23°C | ISO 527-2/5 | 75.0 | MPa |
| Tensile modulus | 23°C | ISO 527-2/5 | 2800 | MPa |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 6.0 | kJ/m² |
| -30°C | ISO 180/1A | 5.0 | kJ/m² | |
| Tensile strain | Break,23°C | ISO 527-2/5 | 35 | % |
| tensile strength | Break, 23°C | ISO 527-2/5 | 75.0 | MPa |
| Tensile modulus | 23°C | ISO 527-2/5 | 2800 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 60.0 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 175 | °C | |
| Melting temperature | ISO 11357 | 223 | °C | |
| Vicat softening temperature | ISO 306/B | 170 | °C | |
| ISO 306/B | 170 | °C | ||
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 60.0 | °C |
| 0.45 MPa, Unannealed | ISO 75-2/B | 175 | °C | |
| Melting temperature | ISO 11357 | 223 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 3.0 | % |
| density | ISO 1183 | 1.13 | g/cm³ | |
| water content | ISO 960 | <2000 | ppm | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 3.0 | % |
| density | ISO 1183 | 1.13 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | IEC 60093 | 1E+15 | ohms·cm | |
| Surface resistivity | IEC 60093 | 1E+13 | ohms | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | ||
| Surface resistivity | IEC 60093 | 1E+13 | ohms | |
| Volume resistivity | IEC 60093 | 1E+15 | ohms·cm | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.