Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ASTMD570 | 2.1 % |
VOCContent | | | <1.0 % |
thermosetting | Test Condition | Test Method | Test Result |
---|
shelf-life | | | 100 wk |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
colour | | | Amber |
density | | | 1.14 g/cm³ |
flash point | | | >100 °C |
| | | 0.20 Pa·s |
Curing Time | | | 0.25 hr |
Cured Properties | Test Condition | Test Method | Test Result |
---|
LinearShrinkage | | | 1.9 % |
hardness | Test Condition | Test Method | Test Result |
---|
| | | 83 |
optical performance | Test Condition | Test Method | Test Result |
---|
refractive index | | | 1.540 |
transparency | | | >98.0 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
TemperatureRange | | | -54到149 °C |
VolumeShrinkage | | | 6.6 % |
nonvolatile content | | | >99 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | | 15.2 MPa |
elongation | Break | ASTMD638 | 3.9 % |
film | Test Condition | Test Method | Test Result |
---|
Elastic modulus MD | | ASTMD882 | 254 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.