PA66 Tislamid® PA66 PA66 25 GFR FR Tisan
0
- Properties:Filler glass fiber reinforced material 25% filler by weight
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/A | 7.0 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Burning wire flammability index | 3.0mm | IEC 60695-2-12 | 960 °C |
| UL flame retardant rating | 1.6mm | UL 94 | V-0 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | Yield | ISO 527-2 | 140 MPa |
| Break | ISO 527-2 | 140 MPa | |
| Tensile strain | Yield | ISO 527-2 | 2.9 % |
| Break | ISO 527-2 | 3.0 % |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/Be | 250 °C |
| Vicat softening temperature | ISO 306/B120 | 255 °C | |
| Melting temperature | 255to260 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | 0.30 % | ||
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 1.8 % |
| ash content | ISO 3451 | 25 % | |
| density | ISO 1183 | 1.55 g/cm³ |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Compared to the anti leakage trace index | 3.00mm | IEC 60112 | PLC 2 |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreD | ISO 868 | 83 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.