Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.28 g/cm³
melt mass-flow rateASTM D123815 g/10min
Shrinkage rateASTM D9550.40to0.70 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTM D785115
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-0
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldASTM D63855.2 MPa
elongationBreakASTM D63840 %
Flexural modulusASTM D7902280 MPa
bending strengthASTM D79079.3 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D256480 J/m
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D64882.8 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.