thermosetting | Test Condition | Test Method | Test Result |
---|
STORAGE STABILITY | | | 9.0 min |
stripping time | | | >60 min |
Post curing time | | | 16 hr |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.15 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
| Shore A | ASTMD2240 | 94到96 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
Dynamic Properties | | | 3.2E+08 dynes/cm² |
Dynamic Properties | | | 2.1E+08 dynes/cm² |
Dynamic Properties | | | 0.0150 |
Dynamic Properties | | | 0.0130 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
compressive strength | | ASTMD695 | 2.76 MPa |
compressive strength | | ASTMD695 | 5.52 MPa |
compressive strength | | ASTMD695 | 8.27 MPa |
compressive strength | | ASTMD695 | 11.7 MPa |
compressive strength | | ASTMD695 | 15.2 MPa |
elastomer | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD412 | 44.8 MPa |
elongation | Break | ASTMD412 | 580 % |
tear strength | Split | ASTMD470 | 25 kN/m |
compression set | | ASTMD395B | 45 % |
compression set | | ASTMD395B | 60 % |
Basho elasticity | | ASTMD2632 | 62 % |
Tensile stress | | ASTMD412 | 10.3 MPa |
Tensile stress | | ASTMD412 | 13.8 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.