PP STERLENE™ RP0100230U R&P (Pte.) Ltd.

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11831.10 g/cm³
melt mass-flow rateISO 11333.0 g/10min
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-2/508670 MPa
tensile strength ISO 527-2/5043.0 MPa
Tensile strainISO 527-2/50<5.0 %
Flexural modulusISO 1786820 MPa
bending strengthISO 17867.0 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180/A5.4 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/Bf149 °C
Heat distortion temperatureISO 75-2/Af118 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.