hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore A | ASTMD2240 | 70 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
BreakingEnergy | 10.8 J | ||
ClashBerg - TF | -41 °C |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile stress | ASTMD412 | 6.01 MPa | |
tensile strength | Yield | ASTMD412 | 15.1 MPa |
elongation | Break | ASTMD412 | 350 % |
aging | Test Condition | Test Method | Test Result |
---|---|---|---|
Change rate of tensile modulus in air | ASTMD573 | 13 % | |
Change rate of ultimate elongation in air | ASTMD573 | 3.0 % | |
Changes in air quality | ASTMD573 | 5.0 % | |
Change rate of tensile strength in air | ASTMD573 | -11 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.