Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD1505 | 1.12 g/cm³ |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTMD1003 | 2.0到4.0 % |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
Film thickness - tested | 51 µm | ||
Secant modulus | ASTMD882 | 827 MPa | |
ASTMD882 | 931 MPa | ||
tensile strength | ASTMD882 | 93.1 MPa | |
elongation | ASTMD882 | 350 % | |
ASTMD882 | 350 % | ||
Elmondov tear strength | ASTMD1922 | 100 g | |
ASTMD1922 | 100 g | ||
tensile strength | ASTMD882 | 93.1 MPa | |
oxygen permeability | ASTMD3985 | 0.55 cm³·mm/m²/atm/24hr |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.