PC ML-3210ZLP TEIJIN JAPAN
106
Form:Granules | Grade:Food grade
Properties:
Weather resistanceAging resistanceHydrolysis resistance
Typical Applications:
Casters
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Casters |
| Properties: | Weather resistance | Aging resistance | Hydrolysis resistance |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Pigment dispersion | 2.0mmt | In-house method | 24 | % |
| Transmittance rate | 1.5mmt | JIS K7136 | 80 | % |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of cantilever beam gap | Notched | ISO 179 | 10 | kJ/m² |
| bending strength | 2mm/min | ISO 178 | 99 | Mpa |
| Bending modulus | 2mm/min | ISO 178 | 2400 | Mpa |
| Elongation at Break | 50mm/min | ISO 527-1 | 105 | % |
| tensile strength | 50mm/min,Break | ISO 527-1 | 68 | Mpa |
| 50mm/min,Yield | ISO 527-1 | 61 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.0mm | UL 94 | V-2 | |
| Hot deformation temperature | TD | ISO 11359-2 | 0.7 | X10-4/℃ |
| 线膨胀系数,MD | ISO 11359-2 | 0.7 | X10-4/℃ | |
| 1.80MPa | ISO 75-1 | 129 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | TD | In-house method | 0.5-0.7 | % |
| MD | In-house method | 0.5-0.7 | % | |
| Dissolving fingers | 300℃ | ISO 1133 | 18 | cm310min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.