Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.02 g/cm | |
Shrinkage rate | ISO 294-4 | 0.8-1.4 % | |
Water absorption rate | ISO 62 | 0.6 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile strain | ISO 527-2 | 28 % | |
ISO 527-2 | 150 % | ||
Charpy Notched Impact Strength | ISO 179/1eA | 8.0 KJ/m | |
ISO 179/1eA | 120 KJ/m | ||
Impact strength of simply supported beam without notch | ISO 179/1eU | No Break | |
ISO 179/1eU | No Break | ||
Tensile modulus | ISO 527-2 | 570 Mpa | |
tensile strength | ISO 527-2 | 31 Mpa | |
ISO 527-2 | 47 Mpa |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | IEC 60250 | 7.00 | |
IEC 60250 | 4.20 | ||
Dielectric loss | IEC 60250 | 0.19 | |
IEC 60250 | 0.11 | ||
Compared to the Leakage Traceability Index (CTI) | IEC 60112 | 600 V | |
Volume resistivity | IEC 60093 | 1E+12 Ohm.cm | |
dielectric strength | IEC 60243-1 | 27 KV/mm |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL94 | HB | |
UL94 | HB | ||
Heat distortion temperature | ISO 75-2B | 115 ℃ | |
ISO 75-2B | 45 ℃ | ||
vicat | ISO 306/A | 170 ℃ | |
melting temperature | ISO 3146 | 173 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.