PA6 A27 GK20 D.T.R ITALY
Properties:
Filler glass fiber reinforced material 20% filler by weight
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | glass fiber reinforced material | 20% | filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 55 | J/m |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Hot filament ignition temperature | IEC 60695-2-13 | 650 | °C | |
| UL flame retardant rating | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ASTM D790 | 3900 | MPa | |
| elongation | Break | ASTM D638 | 15 | % |
| tensile strength | ASTM D638 | 50.0 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 180 | °C |
| Vicat softening temperature | ASTM D15251 | 185 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 85.0 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.26 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | ASTM D257 | 1E+15 | ohms·cm | |
| Surface resistivity | ASTM D257 | 1E+13 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.