PC/ABS 2000EZ BK STYRON TAIWAN
42
Form:Granules | Grade:Injection grade
Typical Applications:
Application in the automotive fieldAutomotive interior equipmentCar dashboard
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Application in the automotive field | Automotive interior equipment | Car dashboard |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| -30°C | 13 | 14.0 | kJ/m² | |
| 23°C | 14 | 40.0 | kJ/m² | |
| Dart impact | 23°C,PeakEnergy | ASTM D3763 | 55.0 | J |
| 23°C,TotalEnergy | ASTM D3763 | 62.0 | J | |
| 23°C | ISO 180/A | 63 | kJ/m² | |
| -30°C | ISO 180/A | 47 | kJ/m² | |
| 16 | ||||
| 23°C | 17 | |||
| -30°C | ASTM D256 | 590 | J/m | |
| 23°C | ASTM D256 | 750 | J/m | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Burning rate | FMVSS302 | <100 | mm/min | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | ISO 178 | 90.0 | Mpa | |
| --10 | ISO 178 | 2400 | Mpa | |
| --9 | ASTM D790 | 2450 | Mpa | |
| elongation | Break | ISO 527-28 | >50 | % |
| crack | ISO 527-2/50 | 90 | % | |
| ASTM D638 | 160 | % | ||
| yield | ISO 527-27 | 4.4 | % | |
| ISO 527-2/50 | 4.5 | % | ||
| crack | ISO 527-2/50 | 47.0 | Mpa | |
| ASTM D638 | 55.0 | Mpa | ||
| yield | ISO 527-25 | 54.0 | Mpa | |
| ISO 527-2/50 | 57.0 | Mpa | ||
| ASTM D638 | 58.0 | Mpa | ||
| 4.00mm, injection molding | ISO 527-2 | 2330 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | ISO 11359-222 | 6.9E-05 | cm/cm/°C | |
| 50°C/h,B50N | ISO 30621 | 124 | °C | |
| 1.8MPa | 1.8MPa | ISO 75-220 | 105 | °C |
| 1.8MPa, unannealed | ISO 75-2/A | 106 | °C | |
| ASTM D648 | 109 | °C | ||
| 0.45MPa | 0.45MPa | ISO 75-219 | 126 | °C |
| 0.45MPa, unannealed | ISO 75-2/B | 130 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| 230°C/3.8kg | ASTM D1238 | 3.7 | g/10min | |
| melt mass-flow rate | 260°C / 5.0kg | ISO 1133 | 18 | g/10min |
| Melt Volume Flow Rate (MVR) | 230°C/3.8kg | ASTM D1505 | 7.00 | cm3/10min |
| Shrinkage rate | ISO 294-4 | 0.50-0.70 | % | |
| Water absorption rate | 23°C,24hr | ASTMD570 | 0.15 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.