Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption - Ejil, 65% RH | | 内部方法 | 1.50 |
Water absorption rate | | ISO 62 | 0.16 % |
Shrinkage rate | | ISO 294-4 | 0.10-0.30 % |
density | | ISO 1183 | 1.64 g/cm³ |
flammability | Test Condition | Test Method | Test Result |
---|
Limiting Oxygen Index | | ISO 4589-2 | 25 % |
UL flame retardant rating | | UL 94 | HB |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTM D256 | 850 J/m |
Impact strength of cantilever beam gap | | ASTM D256 | 110 J/m |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
bending strength | | ISO 178 | 400 Mpa |
Flexural modulus | | ISO 178 | 19000 Mpa |
Tensile strain | | ISO 527-2 | 1.9 % |
tensile strength | | ISO 527-2 | 280 Mpa |
Tensile modulus | | ISO 527-2 | 20000 Mpa |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Compared to the Leakage Tracking Index (CTI) | | IEC 60112 | V |
Dissipation Factor | | IEC 60250 | 0.017 |
dielectric constant | | IEC 60250 | 4.60 |
dielectric strength | | IEC 60243-1 | 31 KV/mm |
Volume resistivity | | IEC 60093 | 1E+13 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Linear coefficient of thermal expansion | | ISO 11359-2 | 1.5E-05 cm/cm/°C |
Heat distortion temperature | | ISO 75-2/A | 230 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.