PP Alloy Propafilm™ RHX200 Innovia Films Ltd.
0
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| gloss | 45° | ASTM D2457 | 110 |
| turbidity | ASTM D1003 | 2.0 % |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Friction coefficient | Itself - Dynamic,外层/外层 | ASTM D1894 | 0.25 |
| Itself - Static,外层/外层 | ASTM D1894 | 0.25 |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | MD:121°C,1分钟 | Internal Method | 4.0 % |
| MD:129°C,1分钟 | Internal Method | 7.0 % | |
| TD:129°C,1分钟 | Internal Method | 1.0 % |
| film | Test Condition | Test Method | Test Result |
|---|---|---|---|
| film thickness | 5100 µm | ||
| Sealing emphasis | Internal Method | 0.14 N/mm | |
| Initial sealing temperature | Internal Method | 93.3to146 °C | |
| Oxygen permeability | 23°C,0%RH | ASTMF1927 | 0.43 cm³·mm/m²/atm/24hr |
| Water vapor permeability | 38°C,90%RH | ASTMF1770 | 3.3 g/m²/24hr |
| consumption | Internal Method | 20.1 m²/kg |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.