PA66 DENISTAT Y 30GC 04

0
  • Properties:
    Filler
    glass
    carbon fiber reinforced material
    30%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.31 g/cm³
Shrinkage rateASTM D9550.50 %
Shrinkage rateASTM D9551.0 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTM D63812000 MPa
tensile strength YieldASTM D638185 MPa
elongationBreakASTM D6382.2 %
Impact resistanceTest ConditionTest MethodTest Result
Suspended wall beam without notch impact strengthISO 18055 kJ/m²
Impact strength of cantilever beam gapISO 180/A8.0 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
Surface ResistivityASTM D2571E+04 ohms
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648A250 °C
vicatASTM D15252250 °C
RTI ElecUL 746140 °C
RTI ImpUL 746140 °C
RTIUL 746140 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.