EPDM Precision Polymer E70K Precision Polymer Engineering Ltd.
0
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Permanent compression deformation | 125°C,24hr | ASTM D395B | 5.0 % |
| 125°C,24hr2 | ISO 815 | 5.0 % | |
| tensile strength | Yield | ASTMD412 | 14.6 MPa |
| elongation | Break | ASTMD412 | 200 % |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Maximum operating temperature | -- | 125 °C | |
| Shorterterm,intermittent | 150 °C |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| IRHD hardness | ASTMD1415 | 74 |
| aging | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Change rate of tensile strength in air | 100°C,70hr | ASTMD412 | -1.0 % |
| Change rate of ultimate elongation in air | 100°C,70hr | ASTMD412 | -11 % |
| Change rate of IRHD hardness in the air | 100°C,70hr | ASTMD573 | 3.0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.