EVA 7140F FPC TAIWAN
194
Form:Granules
Typical Applications:
chipfilmcurrencySanitary products
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | chip | film | currency | Sanitary products |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| gloss | 45°,50.0μm,Blown Film | ASTM D2457 | 90 | |
| turbidity | 50.0μm,Blown Film | ASTM D1003 | 3.0 | % |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield | ASTM D638 | 6.86 | Mpa |
| Break | ASTM D638 | 19.6 | Mpa | |
| elongation | Break | ASTM D638 | 750 | % |
| Bending modulus | ASTM D790 | 22.6 | Mpa | |
| Friction coefficient | Blown Film | ASTM D1894 | 0.50 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Brittle temperature | ASTM D746 | -70.0 | °C | |
| Vicat softening temperature | ASTM D1525 | 75.0 | °C | |
| Melting temperature | 90.0 | °C | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D1505 | 0.934 | g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 0.70 | g/10min |
| Vinyl acetate content | 14.0 | wt% | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreA | ASTM D2240 | 9240 | |
| film | Test Condition | Test Method | Test Result | Test Unit |
| Elmendorf tear strength | TD:50μm,Blown Film | ASTM D1922 | 48 | g |
| Secant modulus | 1%Secant,MD:50μm,Blown Film | ASTM D882 | 36.3 | Mpa |
| 1%Secant,TD:50μm,Blown Film | ASTM D882 | 41.2 | Mpa | |
| tensile strength | MD:Yield,50μm,Blown Film | ASTM D882 | 4.90 | Mpa |
| TD:Yield,50μm,Blown Film | ASTM D882 | 3.92 | Mpa | |
| MD:Break,50μm,Blown Film | ASTM D882 | 30.4 | Mpa | |
| TD:Break,50μm,Blown Film | ASTM D882 | 27.5 | Mpa | |
| elongation | MD:Break,50μm,Blown Film | ASTM D882 | 450 | % |
| TD:Break,50μm,Blown Film | ASTM D882 | 600 | % | |
| Dart impact | 50μm,Blown Film | ASTM D1709 | 620 | g |
| Elmendorf tear strength | MD:50μm,Blown Film | ASTM D1922 | 20 | g |
| film thickness | 50 | µm | ||
| 1.2-5.9mil(30-150µ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.